Abstract

Heat treatment of Pinus pinaster and Eucalyptus globulus woods, two important species in Portugal, was performed in the absence of air by steaming, inside an autoclave, for 2–12 h at 190–210°C. Mass losses increased with treatment time and temperature reaching 7.3% for pine and 14.5% for eucalypt wood. The wood behaviour with moisture was improved. The equilibrium moisture content decreased by 46% for pine and 61% for eucalypt, the dimensional stability increased (maximum anti-shrinking efficiency in the radial direction of 57 and 90% for pine and eucalypt, respectively) and the surface wettability was lowered. In relation to mechanical properties, the modulus of elasticity was little affected (maximum decrease of 5% for pine and 15% for eucalypt) but the bending strength was reduced (by 40% at 8% mass loss for pine and 50% at 9% mass loss for eucalypt wood). The variation of properties was related to treatment intensity and mass loss but significant improvements could already be obtained for a 3–4% mass loss without impairing the mechanical resistance. The response of eucalypt was higher than that of pinewood. Heat treatment of eucalypt wood shows an interesting potential to improve the wood quality for solid timber products.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.