The effects of Strontium (Sr), Iron (Fe) and Manganese (Mn) additions, casting process (i.e., cooling rate) on the microstructures and mechanical properties of AlSi7Cu3 alloy were investigated. 2D and 3D metallographic and image analysis have been performed to measure the microstructural changes occurring at different Sr, Fe and Mn levels and casting process. The evolution of mechanical properties of the alloys has been monitored by Brinell and Vickers hardness measurement and tensile tests. Addition of Sr slightly refines the eutectic silicon particles but it also introduces more pores. The combined addition of Fe and Mn induces an increase of Fe-rich intermetallic compounds which include both α-Al15(Fe,Mn)3Si2 and β-Al5FeSi phase, while the volume fraction of porosity decreases with the Fe and Mn content increase. The secondary dendrite arm spacing slightly decreases with the addition of Sr, Fe and Mn alloying elements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.