Abstract

This study presents the results of systematic variation of essential processing parameters with regard to thermal debinding and sintering of components fabricated by MIM using Ti–6Al–4V powder. The investigation aims at the understanding of the particular influence these parameters have on the mechanical properties of the sintered parts. This study shows that the debinding parameters appear to be rather uncritical, whereas sintering and cooling rates as well as maximum temperature are important in terms of their effect on tensile strength. Contrary to the strength, the ductility remains nearly unaffected. Based on these results, samples displaying yield strength of 757 MPa, UTS of 861 MPa and a plastic elongation of more than 14% were produced. These values meet the requirements of the ASTM B348-02 for titanium alloy grade 23.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.