Abstract

Kaolinitic clays of different varieties were progressively added to a 70: 30 mix of common clay and fly ash. The improvement in physico-mechanical properties upon heating in the temperature range of 1050° to 1200°C was studied by evaluating their linear shrinkage, water absorption, flexural strength and phase content. Incorporation of clay I produced better ceramic properties than that of clay II. It was observed that incorporation of kaolinitic clay up to 10% of the total batch improved the physico-mechanical properties and beyond this limit the properties, particularly fired strength, remained unchanged or marginally decreased. Microstructural features were also studied using SEM technique.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.