The predominant fracture mode during hydrogen assisted environmental failure of 300M steel is intergranular. However, limited attempts have been made to study the failure mode, both as a function of applied stress intensity and as a function of heat treatment. In this investigation, studies were conducted for 300M steel specimens subjected to load in a 3.5% NaCl solution.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Proceedings, annual meeting, Electron Microscopy Society of America
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.