Abstract
The effect of temper temperature and duration on the microstructure and mechanical properties of new-type ultrahigh strength Fe-Ni-Co alloy was investigated with by mechanics performance testing and TEM. The results showed that the maximum ultimate tensile strength could reach 2230MPa after temper near 470°C due to the precipitation of coherent zones of fine carbides. With tempering time extended, the strength was cut down by the M2C carbides coarsening and the decreased coherency with matrix.