Abstract

1. Heat treatment influences the crystal lattice and the saturation of the solid solution of the γ-phase of austenitic manganese cast iron. 2. Regardless of the friction and wear conditions (friction without lubrication or with lubrication containing abrasive) the lattice constant of the heat treated cast iron decreases with increasing pressure and the lattice constant changes in the same way. 3. The more saturated the solid solution before the wear resistance tests, the greater the change in the lattice constant.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.