Red mud lightweight baking-free brick was prepared by red mud, fly ash and cement, mixed with a certain amount of activator agent and foaming agent. The influence of foaming agent on properties of red mud lightweight baking-free brick was studied. The micro-structure of red mud lightweight baking-free brick was characterized by scanning electron microscopy (SEM). The results show that when the foaming agent content is 10ml, the sample with better performance obtained and the density is 423kg/m3, flexural strength is 0.49MPa and compressive strength is 1.87MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.