Abstract

Titanium offers a high specific strength, low density, and excellent corrosion resistance. It finds application in many fields like automotive, aerospace, drilling, and biomedical industries. To improve the adherence of bone cells on implants a rough surface can be of advantage. Such a surface is featured by a foamed structure. For achieving a foamed Ti structure, laser induced foaming was used. In this case, Ti powder is pre mixed with foaming agents. The foaming agents are degraded by laser induced energy and produce gaseous products like carbon dioxide, while the Ti powder is molten by the laser. Due to the fast cooling rate carbon dioxide forms gaseous bubbles in the solidifying material. Mandatory for the foaming agents is that they are biocompatible. Previous studies using the foaming agents CaCO3, MgCO3, MgTiO3, and MgTiO3 mixed to Ti powder resulted in a porosity of up to 0.3. By varying the content of the foaming agent porosity and pore diameter of the samples were adjusted.It is expected that an increased porosity could be achieved by mixing the foaming agents among each other. The influence of the specific foaming agents and their mixtures on the porosity is presented in this work. By mixing the foaming agents together and adding them to the powder, the porosity of the samples was increased compared to only adding one foaming agent to the powder.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.