Hydroxyapatite (HAp) nanocrystals with different levels of fluorine substitution (P/F = 0, 6, 4 and 2) on the OH sites were produced via hydrothermal method. The fluorine substitution was found to alter the morphology of crystals appreciably. The aspect ratio and the crystallinity of HAp crystals increased with increasing fluorine substitution. The presence of broad ring and hallow ring patterns in electron diffraction suggests the low-crystalline nature of HAp crystals. With increasing fluorine substitution, the diffraction patterns exhibited discrete rings and numerous diffraction spots, implying the increased crystallinity. Raman spectra from the HAp nanoparticles also support the less-crystalline nature of the pristine HAp and the enhanced crystallization by fluorine substitution. In HAp crystals processed with no fluorine substitution, surface energy and planar Ca2+ density are less sensitive to the crystallographic orientation because of its low-crystalline nature, favoring equi-axed or slightly elongated particles. The addition of fluorine apparently increased the crystallinity, enhancing the orientation dependent growth and accordingly the aspect ratio. Osteoblast proliferation was observed to be enhanced by fluorine substitution in HAp. In vitro biological data support that the excellent osteoblastic cell viability and functional activity of the fluoridated apatite.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.