Abstract

An experimental investigation on the resistance welding of carbon-fiber-reinforced polyetheretherketone (PEEK) composite laminate using three types of stainless steel (SS) meshes with different sizes and electrical resistances as heating elements is reported. The objective of this study is to determine the influence of the metal mesh on the welding process and performance at different power densities ranging from 29 to 82 kW/m2. Resistance welding equipment is used to monitor the temperature and displacement along the thickness of the laminate. The results show that the power density determines the welding time and heat concentration. A large power density results in a short welding time, but also increases the temperature gradient at the joining interface (almost 50 °C) and causes an obvious deformation of a contraction of more than 0.1 mm along the thickness of the laminate. A SS mesh with low resistance has a strong welding capability, i.e., a high welding efficiency under low power density. A lap shear strength of approximately 35 MPa can be obtained with the appropriate power density. The shear strength is affected by the bonding between the metal mesh and polymer, the metal mesh load bearing, and the metal mesh size.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.