Abstract
Objectives To evaluate the bond strength (μTBS) of self-etching adhesives in different solvent evaporation conditions. Methods Flat dentine surfaces from extracted human third molars were bonded with: (1) 2 two-steps self-etching adhesives (Clearfil SE Bond—CSEB); (Protect Bond—PB) and (2) 2 one-step self-etch systems (Adper Prompt L Pop—ADPLP); (Xeno III—XIII). Bonded dentine surfaces were air-dried for 5 s, 20 s, 30 s or 40 s at either 21 °C or 38 °C. Composite build-ups were constructed incrementally. After storage in water for 24 h at 37 °C, the specimens were prepared for microtensile bond strength testing. Data were analyzed by two-way ANOVA and Student–Newman–Keuls at α = 0.05. Results CSEB and PB performed better at warm temperature with only 20 s of air-blowing. The bond strength increased when XIII was performed at warm temperature at 40 s air-blowing. Extended air-blowing not affect the performance of ADPLP, except at 30 s air-blowing time at warm temperature. Conclusions The use of a warm air-dry stream seems to be a clinical tool to improve the bond strength to self-etching adhesives.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.