Cement Kiln Dust (CKD) is produced as a solid waste with large quantities during manufacturing of Portland cement clinker. The possibility of utilizing CKD as partial replacement for Ordinary Portland Cement (OPC) and White Portland Cement (WPC) produced in factories of the Iraqi cement state company has been examined in this study to fulfil the environmental and economical aims. Different percentages of CKD were blended with OPC and WPC mixes. The results show that the amount of water for normal consistency were increased with about 39 % and 31 % for OPC and WPC blended with 25 % CKD. The setting time (initial and final) decreases with increasing percent of CKD added. Compressive strength decreases slightly with increasing CKD content up to 10 %. For 7- day curing time, it decreases 7 % and 9 % for OPC and WPC mixes, respectively. As percent of added CKD increases to more than 10 %, the compressive strength and other parameters where affected significantly. Overall results proved that OPC and WPC blended with up to 10 % CKD are admissible for passing relevant specification requirements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.