Development of synthetic bone graft via bone tissue engineering involves seeding of patient’s stem cells onto a porous scaffold in presence of growth factors. Porosity, strength and dimensional accuracy of the porous scaffold play a vital role in this process. This work aims at ascertaining influence of build orientation on porosity, mechanical strength and dimensional accuracy of the selectively laser sintered polyamide porous scaffolds. Initially, CAD models of test specimens with pre-designed porosity were created in Solidworks® software. All the specimens were fabricated on EOSINT P395, a selective laser sintering machine, along various primary (Flat, Edge, Upright and Flat_diag) and secondary (0o, 30o, 45o, 60o and 90o) orientations. Results show that measured porosity of most of the specimens was (range: 42.89-35.26%) less than the designed porosity (41.71%). Maximum average tensile strength (16.84 MPa) was recorded for specimens printed along Flat_0o orientation. Specimens printed along Upright_90o orientation showed highest average compressive strength (8.26 MPa). Specimens printed along Flat orientation showed relatively better average impact strength. Best dimensional accuracy was obtained for specimens printed along Flat orientation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.