Indium is one of the key components in an LCD. In this work a potential recycling method involving leaching and solvent extraction was studied. Leaching of crushed LCD glass was investigated using HCl, HNO3, or H2SO4. Results of leaching kinetics showed that nearly complete leaching of indium can be achieved using 1M HCl and 1M H2SO4 in less than 8h. A screening test was performed for the extraction and separation of indium from HCl or H2SO4 with DEHPA, TBP, and Cyanex 272 or Cyanex 923. More than 99% of indium from the aqueous feed can be recovered with a purity of 90%, by extracting metal ions from 1M or 0.1M H2SO4 to 0.1M DEHPA diluted in kerosene, and back-extracting with 1M HCl.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.