Coal-fired power plants produce flue gas desulfurization (FGD) gypsum as a byproduct of the sulfur removal process. This gypsum is contaminated with trace elements. Knowing the occurrence and release characteristics of trace elements from the FGD gypsum is very important if the gypsum is to be safely used in different applications. The sequential extraction procedure proposed by the European Community Bureau of Reference (BCR) can be used to provide mercury speciation information for FGD gypsum samples. Many researchers have used the BCR sequential extraction method to analyze the occurrence of mercury in FGD gypsum. Unfortunately, the recovery ratio is low, around 50–60%. The recovery is low because the BCR method does not include the portion of elemental mercury (Hg0) lost during each leaching step. In this work, modifications to the BCR method were made to more accurately determine the amount of mercury lost during the extraction. Using this “improved BCR method”, the Lumex RA-915+/PYRO-915 mercury ana...
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have