Abstract

A novel heap leaching method was investigated for selective removal of chromium (Cr) and vanadium (V) from ferrochromium (FeCr) and stainless steel (SS) slags. In particular, alkaline oxidative heap leaching was simulated on lab-scale by batch and column leaching tests. The results show a selective leaching of Cr (11–19%) and V (7.0–7.5%) after 64days of column leaching, with a very low dissolution (<2.2% (FeCr slag) and <0.15% (SS slag)) of matrix elements (e.g. Al, Fe, Si, Mg, Ca), when NaOCl is applied as oxidation agent and NaOH as alkaline agent. Furthermore, the used leaching liquor is reactive for a longer period of time, indicating that circulation of leaching liquor could be possible. Finally, the experimental results were fed into a first-order model which predicts that Cr will continue to leach from the tested slags for 4–5years at a chosen infiltration rate of 73,000 l/(ym2).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.