Abstract

Fe–Si alloys are an essential class of soft magnetic materials due to their high magnetic permeability and low hysteresis loss. Increasing the Si content above 3 wt% promotes coarser grain sizes and greater electrical resistivity, thereby enhancing the magnetic properties, such as magnetic permeability and specific loss density. However, the increased silicon content makes the machining challenging. Additive manufacturing technologies enable production of near net shape Fe–Si alloys with high silicon content, practically eliminating the machining challenges. This work investigated the effects of Si content, which ranged from 3 to 5 wt%, and B content, which ranged from 0 to 0.25 wt%, on the microstructure and magnetic properties. The Fe–Si–B alloys were binder jet printed, where the sintering temperature was varied between 1200 and 1250 °C, and microstructure-magnetic property relationships were investigated by characterizing the magnetic permeability, intrinsic coercivity, grain size, and density. The Fe-5wt.%Si alloy with 0.25% B sintered at 1200 °C exhibited the highest magnetic relative permeability (4447) and the lowest intrinsic coercivity (47.8 A/m).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.