Improving Intergranular Stress Corrosion Cracking Resistance in a Fe–18Cr–17Mn–2Mo–0.85N Austenitic Stainless Steel Through Grain Boundary Character Distribution Optimization

Publication Date Jul 9, 2022

Abstract

Improving Intergranular Stress Corrosion Cracking Resistance in a Fe – 18Cr – 17Mn – 2Mo – 0.85 N Austenitic Stainless Steel Through Grain Boundary Character Distribution Optimization

Concepts

Intergranular Stress Corrosion Cracking Resistance Austenitic Stainless Steel Intergranular Corrosion Intergranular Cracking Intergranular Stress Corrosion Cracking Stress Corrosion Cracking Resistance Boundary Character Distribution Corrosion Cracking Resistance Stress Corrosion Intergranular Stress

Round-ups are the summaries of handpicked papers around trending topics published every week. These would enable you to scan through a collection of papers and decide if the paper is relevant to you before actually investing time into reading it.

Climate change Research Articles published between Sep 12, 2022 to Sep 18, 2022

R DiscoverySep 19, 2022
R DiscoveryArticles Included:  5

Rainfall projections from the Coupled Model Intercomparison Project (CMIP) models are strongly tied to projected sea surface temperature (SST) spatial...

Read More

Coronavirus Pandemic

You can also read COVID related content on R COVID-19

R ProductsCOVID-19

ONE PROBLEM . ONE PURPOSE . ONE PLACE

Creating the world’s largest AI-driven & human-curated collection of research, news, expert recommendations and educational resources on COVID-19

COVID-19 Dashboard

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on “as is” basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The Copyright Law.