Abstract

An applicable method to improve the tensile properties of 2219-T8 aluminum alloy TIG welding joints is attractive in manufacturing of large propellant tanks. In this work, tensile properties of 2219-T8 TIG welded joints was improved by adjusting the weld geometry using multi -pass welding with swing. The effects of weld geometry on the tensile properties of joint were investigated. And the geometry parameters were optimized by an orthogonal experiment design. The joints with tensile strength coefficient of 70 % and elongation over 4% were acquired after weld geometry optimization. The improvement mechanisms of weld geometry attributed to the reduced strain variation rate and stress concentration at the weld toe.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.