Abstract

The use of ITO interlayers between Ga2O3 and Ti/Au metallization is shown to produce Ohmic contacts after annealing in the range of 500–600 °C. Without the ITO, similar anneals do not lead to linear current–voltage characteristics. Transmission line measurements were used to extract the specific contact resistance of the Au/Ti/ITO/Ga2O3 stacks as a function of annealing temperature. Sheet, specific contact, and transfer resistances all decreased sharply from as-deposited values with annealing. The minimum transfer resistance and specific contact resistance of 0.60 Ω mm and 6.3 × 10−5 Ω cm2 were achieved after 600 °C annealing, respectively. The conduction band offset between ITO and Ga2O3 is 0.32 eV and is consistent with the improved electron transport across the heterointerface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.