Abstract
The creep behavior of a novel Ni-based wrought superalloy with varying aging states, classified as large under-aged (UA), little UA, and little over-aged (OA) states, was investigated at a temperature higher than the intra-grain/grain-boundary iso-strength temperature (750 °C/250 MPa). In the samples before creep test, there are spherical γ′ precipitates homogeneously dispersed within the γ matrix and carbides precipitated at grain boundaries (GBs). After creep tests, precipitate-free zones (PFZs) appear on grain boundaries, with a large block-like γ′ phase present between carbides and PFZs, potentially serving as initiation sites for cracks. Little UA state samples exhibit the strongest creep resistance and intergranular fracture. The dominant creep deformation mechanism in the intra-grain is a combination of Orowan process involving slip and climb of matrix dislocations and shearing of γ′ precipitates. The results indicate that the optimizing the grain boundary microstructure may be more important than the change of intragranular microstructure when the creep temperature exceeds the iso-strength temperature.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have