Abstract
The dynamic yield and fracture stress of two refractory alloys were measured under shock-wave loading at normal and elevated (up to 680°C) temperatures. The tested materials were polycrystalline nickel-based superalloy Inconel IN738LC and PWA 1483 Ni–Co–Fe alloy in quasi-monocrystalline state. Both alloys are used as turbine blade materials for the hot first stages of gas turbines. The alloys exhibit non-monotonous dependence of the dynamic yield strength upon temperature with an abrupt increase in the temperature interval of 550–600°C. The dynamic tensile strength, in general, is less sensitive to temperature and shows less pronounced increase in the vicinity of 570°C. The observed anomalies of the dynamic strength properties correlate with anomalies in the heat capacity which are associated with the equilibrating of the short-range order in the γ-matrix of the alloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.