Abstract

OBJECTIVE:This study aimed to assess the feasibility of reusing nickel–titanium (NiTi) alloy wires after 6 weeks of intraoral use by evaluating the changes in the load-deflection properties and surface characterization of these alloy wires after cold sterilization by immersion in 2% of acidic glutaraldehyde for 10 h.MATERIAL AND METHODS:Twenty wires each in three groups of G1-as-received wires (ARW), G2-unsterilized used wires, and G3-sterilized used wires (SUW) were tested by the three-point bending test and scanning electron microscopy (SEM). The data were subjected to statistics, one-way analysis of variance, and Bonferroni posthoc test for comparison.RESULTS:Recycling of NiTi wires produced statistically insignificant changes in both the loading and unloading properties of the wires. The forces needed to twist the used wires, that is, G2-(UUW) and G3-(SUW) were lower than G1-(ARW), suggesting lowering of the stiffness of the wires. Superelasticity is well-maintained by G2-(UUW) and G3-(SUW) although there is an insignificant lowering of the forces exerted by them during loading and unloading. SEM demonstrated no increase in the pitting of surfaces in both G2-(UUW) and G3-(SUW); multiple areas were seen to be more smoothened over G2-(UUW) and G3-(SUW) NiTi wires surfaces.CONCLUSION:The findings of this study support the reuse of NiTi wires after 6 weeks of use in oral conditions followed by cold sterilization by immersion in 2% acidic glutaraldehyde for 10 h.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call