Abstract
The study of grown Sc2SiO5 : Gd and Sc2SiO5 : Fe crystals was carried out by the paramagnetic resonance method. It has been established that Fe3+ ions replace Sc3+ in both crystallographic positions, while Gd3+ ions exhibit a single center localized in a larger position with a coordination number of 7. Measurement of the orientational behavior of the positions of transitions of Fe3+ and Gd3+ centers in two orthogonal planes made it possible to determine the parameters of their triclinic spin Hamiltonians. To determine the localization of impurity ions Cr3+, Fe3+ and Gd3+ in scandium and yttrium silicates, the orientation of the main Z axes of the fine structure tensors of the second rank was used. Keywords: scandium and yttrium silicates, impurity ions, paramagnetic resonance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.