Abstract

HZSM-5 was treated with ammonia water vapor at 373 and 473K, and the catalytic activities for alkane cracking were evaluated. The treatment removed a fraction of silicon from the framework, but the meso-pore was not generated and the micro-pore volume was decreased. The solid acidity was characterized by infrared/mass spectroscopy-temperature programmed desorption (IRMS-TPD) of ammonia experiment. Two kinds of Brønsted acid sites were observed on the unmodified HZSM-5, and the solid acidity did not change largely by the treatment. Catalytic cracking of hexane and octane was enhanced by the treatment, and the second order reaction of cracking became accompanied with the first order reaction. From the products distribution in the propane cracking, the proceeding of bimolecular reaction was confirmed. Discussion was made on the morphology change of the modified HZSM-5 and the resulting enhanced cracking activity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.