Abstract

Gadolinium aluminate (GdAlO3, GAP) nano whiskers were synthesized by the hydrothermal-solid state method, Fourier-transform infrared (FTIR), X-ray diffraction (XRD), scanning electron microscope (SEM) and thermogravimetry-differential thermal analysis (TG-DTA) were employed to analyze the phase change and the nucleation mechanism of GAP during calcing process. The results show that the precursor of GAP prepared by hydrothermal is (NH4)xGdAl(OH)y(NO3)z·nH2O. When the calcination temperature is higher than 900 °C, the precursor recrystallizes, forming the needle shape GAP under the synergistic effect factors. The best preparation conditions are as follows: ammonia water as mineralizer, pH = 9, calcination temperature 1100 °C and holding time 3 h.