Abstract
Hydroisomerization of <i>n</i>-Pentane over Zn-Fe-S<sub>2</sub>O<sub>8</sub><sup style="margin-left:-6px;">-2</sup>/ZrO<sub>2</sub>-Al<sub>2</sub>O<sub>3</sub> Superacid Catalyst: Activity, Surface Analysis and the Investigation of Deactivation and Regeneration