Abstract In the absence of H2S and with the addition of inlet H2S content 719 ppm for 4 hours, 8 hours and 12 hours respectively, the global reaction rates of methanol decomposition were determined over φ 5×5 mm cylindrical pellet of C207 Cu -based catalyst at atmospheric pressure in an internal recycle gradientless reactor. The pore size distribution, the profile of sulfur in pellet, and the tortuosity factor of the poisoned catalyst were also measured. The hydrogen sulfide poisoning of commercial catalyst was considered as the shell-progressive poisoning. The experimental values of the non-poisoned dimensionless radius xc by Auger Electron Spectroscopy were 0·938, 0·916 and 0·896 respectively with the addition of H2S for 4 hours, 8 hours and 12 hours, which were in agreement with the values calculated by the intrinsic deactivation kinetics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.