The hydrogen absorption rate for nickel-ion-plated niobium was measured as a function of hydrogen pressure and temperature. The observed absorption curves of c ̄ c e against time ( c ̄ and c e are the mean and equilibrium hydrogen concentrations respectively) exhibited a marked hydrogen pressure dependence below 628 K but this was less marked above 723 K. The results were analysed on the basis of the proposed model that the rate-determining step is the hydrogen permeation through the nickel overlayer and that the permeation is driven by the hydrogen activity difference between the two interfaces, namely the H 2-Ni and Ni-Nb interfaces. The marked pressure dependence can be attributed to the fact that the hydrogen activity coefficient in nickel is constant and that in niobium it varies markedly with concentration, i.e. with hydrogen pressure and temperature. It was also found that the change in the nickel overlayer structure caused by the dilatation of bulk niobium during hydrogen absorption enhances the hydrogen absorption rates. The temperature dependence of the hydrogen absorption rate is also discussed in comparison with that for tantalum with a vacuum-deposited nickel overlayer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.