Abstract

The effect of hot isostatic pressing in 5°%,O 2 -95%Ar on the magnetic properties of Sr ferrite magnet was studied. It was found that the size of voids at grain boundaries are decreased by hot isostatic pressing without substantial grain growth and the density of isostatically hot-pressed body is about 5.03x10 3 kg/m 3 . Magnetic measurement revealed that the hot isostatic pressing does not signiticantly decrease coercive force and keeps the good squareness of B-H curve of pre-sintered body unchanged. The typical value of residual flux density Br of the isostatically hot-pressed magnet is 0.438T at MHe=318KA/m.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.