Density and correct diameter of nuclear fuel pellets are usually achieved by sintering and subsequent circular grinding. Hot impact densification (HID) thermally squatted ceramic bodies can be directly high speed precision-molded in a cold die. For thermoshock-sensitive materials, a controlled cooling down procedure of some minutes is added. The feasibility of HID has been demonstrated on the laboratory scale on UO/sub 2/, UC, and some more materials at temperatures between 1700 and 2300/sup 0/C, pressures up to 800 N/mm/sup 2/. Shape tolerances are close, density can be exactly reproduced within a wide range. Tool wear seems to be no problem. Currently, a prototype facility for continuous performance is being developed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.