Abstract

Increasing the temperature of HCBS during wet milling makes it possible to obtain a significant reduction of the anomaly of viscosity (for dilatant, thixotropic-dilatant and thixotropic systems), to decrease the volume of the solvated liquid, and to increase the solubility of the solid phase. All these facts permit one to carry out the milling process at a high concentration and to increase the strength of the ceramic binders.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.