Abstract

The MA-SPS (mechanical alloying followed by spark plasma sintering) process was adopted to further improve the high temperature properties of a newly developed 36Cr white cast iron (a eutectic Fe-36Cr-9Ni-5Mo-0.45Si-2.2C alloy). α-Al2O3 powder with a mean diameter of 0.4μm was used as reinforcement for the MA material, and the volume fractions of Al2O3 in the composites were 10% and 30%. The results show that the microstructures of the MA materials were greatly refined compared to those of the conventionally solidified ingot and that their high temperature hardness and high temperature abrasive resistance were considerably improved. Also found was that the increase in the volume fraction of the Al2O3 powder increased both the hardness and the abrasive resistance of the composite materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.