Abstract
AD730™ Ni-based superalloy specimens in solution-treated conditions were linear friction welded. Then, post-weld heat treatment (PWHT), consisting of γ′ sub-solvus solution treatments followed by aging, was conducted on the linear friction welded samples. High temperature creep tests were performed on the as-welded and PWHTed joints at two different temperatures: 700°C under 600 and 750MPa stress levels, and 850°C under 100 and 200MPa stresses. The creep resistance of the PWHTed joints was higher than that of the as-welded samples. The PWHTed joints exhibited better ductility than that of the base material at 850°C, while they showed slightly lower creep life at 700°C in comparison to the base metal. Microstructure examination showed that cracks initiated at the interface of oxidized particles at 700°C. The decrease in creep resistance of the AD730™ Ni-based superalloy at 850°C was related to a combination of the formation of precipitate-free zones (PFZ) in the vicinity of the grain boundaries (GBs) and microcracking assisted by oxidation. The Larson-Miller Parameter (LMP) was used to correlate the creep strength, temperature and time to failure for the as-welded and PWHTed samples. LMP values varied between 21.5 × 103 and 24.5 × 103. It was found that in the investigated temperature range, the PWHTed AD730™ has similar creep characteristics as Udimet™720 Li and Inconel 738LC at low values of LMP and better creep properties than those of the Inconel 617 alloy at higher LMP values.
Accepted Version (Free)
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have