Abstract
In this work, IN738 superalloy used previously in gas turbines was recycled and used as a working electrode for the electrooxidation of different fuels, namely ethylene glycol, ethanol, and urea. The electrocatalytic efficiency of the electrode was studied by cyclic voltammetry, chronoamperometry, and electrochemical impedance. Several kinetics parameters like diffusion coefficient, Tafel slope, rate constant, and activation energy were calculated. The modified electrode was characterized as received using XRD, SEM, and EDAX to elucidate the crystal structure and surface morphology before and after electrochemical oxidation. The anodic current densities of electrochemical oxidation of ethanol, ethylene glycol, and urea were 29, 17, and 12 mA.cm−2, respectively, in an alkaline solution at a potential of 0.6 V (vs. Ag/AgCl). The kinetic parameters like diffusion coefficients for ethanol, ethylene glycol, and urea were found to be 1.5 times 10–6, 1.038 times 10–6, and 0.64 times 10–6 cm2 s−1, respectively. The charge transfer resistances were estimated for electrooxidation of different fuels by electrochemical impedance spectroscopy (EIS).Graphical
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have