Abstract
Nanocrystalline diamond (NCD) is increasingly popular as engineered surface coatings intended for tribo-mechanical applications. Sliding may occur in the presence of water, or aqueous solutions, for example in mechanical face seals, MEMS, or in preliminary testing bearing surfaces for biotribological applications. NCD coatings of 20 μm thickness were grown by the hot-filament chemical vapour deposition (HFCVD) method on Si 3N 4 ceramic substrates. The water lubricated NCD/NCD tribosystem was studied in an oscillating ball-on-flat tribometer. For all loading conditions up to the threshold load prior to film delamination (85 N), very low friction coefficient values ( μ ∼ 0.02 to 0.05) combined with a high wear resistance (10 − 9 to 10 − 8 mm 3N − 1m − 1) were observed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.