The purpose of this study was to investigate the effect of heat treatment (930°C, 1080°C, 1230°C) followed by quenching on the pitting corrosion resistance, sigma phase precipitation, and microstructural change of a super duplex stainless steel (UNS S32750) welds made by gas tungsten arc (GTA). Based on the microstructural examination, the σ phase was formed in welds heat treated at 930°C while there were little σ phases formed in welds experienced the relatively fast cooling from 1080°C and 1230°C. Accordingly, the most weight loss due to pitting corrosion occurred in the as received base and weld metals heat treated at 930°C. It was confirmed that the pitting corrosion occurred in the phase boundaries of ferrite/sigma and austenite/sigma.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.