Abstract

Stoichiometric nano-hydroxyapatite is synthesized and compacted by UP (Uniaxial pressing) and CIP (Cold isostatic pressing). It is sintered (S) and subsequently is immersed in SBF (Synthetic body fluid). Hardness and roughness are analyzed in each part of process. The relationship between hardness and roughness is proportional after UP. While in the CIP and sintering the relationship is symmetric with a maximum. After immersion there is no clear functional relationship. Roughness changes at each stage of the process are -13.3% (UP → CIP), 22.10% (CIP → S) and -61.5% (S → SBF), respectively. Analogously, for area particle: 405.60%, 120.20% and -99.8%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.