Abstract

The aim of this study was to determine the hardening effect by controlling the cooling rate during the porcelain firing process and performing an additional post-firing heat treatment in a Pd-Ag-Sn alloy. The most effective cooling rate for alloy hardening was determined by cooling the specimens at various cooling rates after oxidation treatment. A subsequent porcelain firing simulation followed by cooling at the selected cooling rate was performed. A post-firing heat treatment was then done at 600°C in a porcelain furnace. The hardening mechanism was characterized by a hardness test, X-ray diffraction, field emission scanning electron microscopy and energy dispersive X-ray spectroscopy. Alloy softening occurred during the porcelain firing process followed by cooling at a controlled cooling rate. A post-firing heat treatment allowed apparent precipitation hardening. It is advisable to perform a postfiring heat treatment at 600°C in a porcelain furnace by annealing metal substructure after porcelain fusing.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call