Abstract
Growth, spectroscopy and diode-pumped laser operation of acentric Yb:KGd(PO<sub>3</sub>)<sub>4</sub> crystal
Highlights
The doping concentration was measured by electron probe microanalysis, NYb = 1.0×1020 cm-3 (2.4 at.% Yb)
P21) and optically biaxial [2]
The Ng-cut uncoated crystal was 7.03 mm-thick; it was mounted in a Cu-holder cooled by flowing water (14 °C)
Summary
The doping concentration was measured by electron probe microanalysis, NYb = 1.0×1020 cm-3 (2.4 at.% Yb). P21) and optically biaxial (it is phase-matchable for type I second harmonic generation) [2].