Abstract

The band alignment of ultrathin ZrO2 films of different thickness formed on Si(100) have been monitored with synchrotron radiation photoelectron spectroscopy and x-ray absorption spectroscopy. The films were deposited sequentially by way of metal-organic chemical-vapor deposition in ultrahigh vacuum. A significant decrease in the conduction band offset is found for increasing film thickness. It is accompanied by a corresponding increase of the valence band offset. The variations originate in the formation of an interfacial layer characterized by a lower degree of Zr-O interaction than in bulk ZrO2 but with no clear evidence for partially occupied Zr4d dangling bonds.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.