This work suggested the growth of SiC and SiO2nanostructures from heating of rice husk ash and carbon-metal assisted. The rice husk was boiled in 1 M hydrochloric acid solution with temperature of around 90 °C for 1 hour, and then washed in distilled water and dried under the sun. The dried acid-treated rice husk was burned in the furnace with normal air for 1 hour, then high purity SiO2was produced. The high silica ash mixed with Cu or SnO2powder and coconut shell charcoal were grounded for mixtures powder. The mixtures powder and Si substrates were placed on the alumina boat and put in the middle of furnace. The furnace was heated at high temperature under atmosphere of argon gas. The heated products and Si substrates were studied by X-rays diffraction and scanning electron microscope. The SiC and SiO2nanostructures were observed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.