We have analyzed conditions for the growth of large (≥80 mm in diameter) LiNbO3〈Mg〉 crystals in a wide range of dopant concentrations in the melt (2.9–5.8 mol % MgO). We have established conditions for the growth of large LiNbO3〈Mg〉 crystals uniform in doping level from melts containing magnesium concentrations above a certain threshold (Cmelt 5.0–5.8 mol % MgO) and optimized the high-temperature electrodiffusion annealing process, which allowed us to obtain single-domain, microstructurally homogeneous, large LiNbO3〈Mg〉 crystals containing 4.9–5.15 mol % magnesium.