Abstract

(KNa)0.1(Sr0.6Ba0.4)0.9Nb2O6, or KNSBN, crystals have been grown with two different Mn concentrations: 0.02 wt % and 0.04 wt %. Two-wave mixing and self-pumped phase conjugation experiments were carried out on these crystals at 632.8 nm wavelength. The measured two-wave coupling gains for the 0.02 wt % and 0.04 wt % crystals are larger than 7 cm−1 and 9 cm−1, respectively, and the two-wave coupling time response is faster for the 0.4 wt % crystal. In addition, the self-pumped phase conjugation reflectivity of the 0.04 wt % crystal is measured to be as high as 70%. It is shown that the Mn dopant can increase effectively the absorption coefficient and enhance the photorefractive properties of KNSBN.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.