Abstract

Thiocyanate (SCN–) is a promising alternative to cyanide as a lixiviant for gold extraction and is 1000 times less toxic than cyanide. In this study, the following leaching parameters were tested to optimize the gold recovery for the first time from an oxide ore using the response surface methodology: initial thiocyanate concentration (10–500 mM), initial Fe3+ concentration (10–500 mM), and pulp density (10–50% w/v). The maximum gold recovery (96%) was achieved with 500 mM thiocyanate, 100 mM Fe3+, and 50% pulp density at 25 °C and pH = 2 for 24 h. A kinetic study on the optimum leaching condition showed that it followed the shrinking core model, in which the rate-controlling mechanism was the diffusion process. These results are discussed in the context of the published literature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.