Containerless melting was employed to evaluate the influence of increasing ZrO2 additions on the glass-forming ability of peraluminous melts in the magnesium aluminosilicate system. The saturation limit of this oxide in glasses along the silica-cordierite join (SiO2–Mg2Al4Si5O18) is inversely proportional to the SiO2 content; however, a limited solubility of ZrO2 in melt-quenched silica exists (∼2 mol%). Peraluminous samples (particularly MgO-free samples) exhibited a substantially higher capability of incorporating ZrO2 without undergoing devitrification during cooling. TEM investigations revealed phase separation in all amorphous samples off the MgO = Al2O3 line, with ZrO2 preferentially segregating into a SiO2-depleted phase. These results identify the key role of Al2O3 for the structural incorporation of ZrO2 in silicate melts, opening up alternative pathways for the development of glasses and glass-ceramics respectively based on the homogeneous distribution of ZrO2 or, in turn, on its exploitation to induce phase separation and crystal nucleation.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call