The Gibbs Free Energy Difference between the solid and liquid phases (DG) is related to nucleation frequency and has played an important role in predicting the glass forming ability (GFA) of multicomponent metallic alloys. This is due to the fact that the maximum energy for nucleus formation i.e. the activation barrier for nucleation has an inverse square relation with DG. The Gibbs Free Energy Difference of three multi-component bulk metallic glasses namely Mg65Cu25Y10, Zr57Cu15.4Ni12.6Al10Nb5 and Zr52.5Cu17.9Ni14.6Al10Ti5 have been evaluated using two new expressions. The results show that the DG values calculated assuming DCp to be constant lie closer to the experimental values for the Mg based system while in the case of two Zr based systems, DG computed using the hyperbolic variation of DCp show improved agreement with the experimental data.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.