Abstract

AbstractThe paper investigates the freeze–thaw resistance and sorptivity behavior of fine‐grained alkali‐activated concrete cured at ambient temperature. A blended binder system containing fly ash, ground granulated blast furnace slag, and silica fume was used. A combination of sodium hydroxide and sodium silicate was used as an activator. The freeze–thaw resistance was evaluated based on mass loss (scaling), and the extent of internal damage was assessed by testing the ultrasonic time at different cycles. Initial and secondary sorptivity coefficients were calculated based on the cumulative water absorption values at different time intervals. Alkali content, sodium silicate to sodium hydroxide ratio, and water to binder ratio were investigated. The experimental results showed that water to binder ratio is the most significant parameter for the scaling; higher ratios result in higher scaling. In terms of internal damage, alkali content is the most significant. The increase of alkali increased the amount of internal damage in the concrete. The initial sorptivity coefficient increased with the water and alkali content and decreased with the silicate content. The secondary sorptivity coefficient showed no significant change with the investigated parameters.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.