Abstract
The free-radical bulk polymerization of lauryl methacrylate (LMA) in the presence of 2,2'-azobisisobutyronitrile (AIBN) has been studied by differential scanning calorimetry (DSC) in dynamic and isothermal modes. The measured heats of reaction Δ H, increased with the concentration of the initiator. The enthalpy of polymerization in the presence of a large excess of AIBN was obtained by extrapolation. At low concentrations of AIBN, a constant heat of polymerization of LMA (−41.7kJ mol −1) was obtained after correcting for both the incomplete conversion to polymer and the decomposition enthalpy of AIBN.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.